Abstract

Objective. The aim of this study was to evaluate the effect of decontamination methods on shear bond strength of resin cement to translucent monolithic zirconia. Material and Methods. Eighty 4-mol yttria-stabilized tetragonal zirconia polycrystal specimens were fabricated. All specimens were subjected to saliva contamination and divided into four groups (n=20) according to the decontamination methods: 70% isopropanol (AL); zirclean (ZC); 5.25% sodium  ypochlorite (NaOCL); and no cleaning (NC). All specimens were bonded by using self-adhesive resin cement. Half of the specimens in each group (n=10) were subjected to thermocycling. All specimens were subjected to shear bond strength test in a universal testing machine. Failure modes were evaluated by using a scanning electron microscope (SEM). The data obtained were statistically analyzed by using one-way ANOVA followed by the HSD Tukey test (P < 0.05). ResultsANOVA test revealed a significant difference among the different decontamination methods (P < 0.05). No significant differences were found among NaOCL, ZC, and AL groups as revealed by the HSD Tukey test (P > 0.05). The effect of thermocycling was significantly different in all groups (P < 0.05); whereas, no significant difference was found in group ZC (P > 0.05). (SEM) analysis showed mixed failures in all groups except in group NC where only adhesive failure was observed. Conclusion. Saliva contamination during clinical evaluation significantly decreases the shear bond strength between self-adhesive resin cement and translucent monolithic zirconia. The cleaning gel has an impact on improving the bond strength between resin cement and translucent monolithic zirconia.  

KEYWORDS

Monolithic zirconia; Resin cement; Shear bond strength test; Translucent zirconia; Zirclean.

References

Miyazaki T, Nakamura T, Matsumura H, Ban S, Kobayashi Current status of zirconia restoration. J Prosthodont Res. 2013 Oct;57(4):236-61. doi: 10.1016/j.jpor.2013.09.001.

Stober T, Bermejo JL, Rammelsberg P, Schmitter M. Enamel wear caused by monolithic zirconia crowns after 6 months of clinical use. J Oral Rehabil. 2014 Apr;41(4):314-22. doi: 10.1111/joor.12139.

Sulaiman TA, Abdulmajeed AA, Donovan TE, Ritter AV, Vallittu PK, Närhi TO, Lassila LV. Optical properties and light irradiance of monolithic zirconia at variable thicknesses. Dent Mater. 2015 Oct;31(10):1180-7. doi: 10.1016/j.dental.2015.06.016.

Ghodsi S, Jafarian Z. A review on translucent zirconia. Eur J Prosthodont Restor Dent. 2018 May 30;26(2):62-74. doi: 10.1922/EJPRD_01759Ghodsi13.

Mao L, Kaizer MR, Zhao M, Guo B, Song YF, Zhang Y. Graded ultra-translucent zirconia (5Y-PSZ) for strength and functionalities. J Dent Res. 2018 Oct;97(11):1222-1228. doi: 10.1177/0022034518771287.

Alraheam IA, Donovan TE, Rodgers B, Boushell L, Sulaiman TA. Effect of masticatory simulation on the translucency of different types of dental zirconia. J Prosthet Dent. 2019 Oct;122(4):404-409. doi: 10.1016/j.prosdent.2019.02.002.

Nassary Zadeh P, Lümkemann N, Sener B, Eichberger M, Stawarczyk B. Flexural strength, fracture toughness, and translucency of cubic/tetragonal zirconia materials. J Prosthet Dent. 2018 Dec;120(6):948-954. doi: 10.1016/j.prosdent.2017.12.021.

Vult von Steyern P, Carlson P, Nilner K. All-ceramic fixed partial dentures designed according to the dc-zirkon technique. A 2-year clinical study. J Oral Rehabil. 2005 Mar;32(3):180-7. doi.org/10.1111/j.1365-2842.2004.01437.x.

Sailer I, Pjetursson BE, Zwahlen M, Hämmerle CH. A systematic review of the survival and complication rates of all ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part II: Fixed dental prostheses. Clin Oral Implants Res. 2007 Jun;18 Suppl 3:86-96. doi.org/10.1111/j.1600-0501.2007.01468.x.

Tinschert J, Schulze KA, Natt G, Latzke P, Heussen N, Spiekermann H. Clinical behavior of zirconia-based fixed partial dentures made of DC-Zirkon: 3-year results. Int J Prosthodont. 2008 May-Jun;21(3):217-22.

Rinke S, Fischer C. Range of indications for translucent zirconia modifications: clinical and technical aspects. Quintessence Int. 2013;44(8):557-66. doi: 10.3290/j.qi.a29937.

Kim MJ, Kim YK, Kim KH, Kwon TY. Shear bond strengths of various luting cements to zirconia ceramic: surface chemical aspects. J Dent. 2011Nov;39(11):795-803. doi: 10.1016/j.jdent.2011.08.012.

Blatz MB, Alvarez M, Sawyer K, Brindis M. How to bond zirconia: The APC concept. Compend Contin Educ Dent. 2016 Oct;37(9):611-617; quiz 618.

Yang B, Barloi A, Kern M. Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin. Dent Mater. 2010 Jan;26(1):44-50. doi: 10.1016/j.dental.2009.08.008.

Inokoshi M, Kameyama A, De Munck J, Minakuchi S, Van Meerbeek B. Durable bonding to mechanically and/or chemically pre-treated dental zirconia. J Dent. 2013 Feb;41(2):170-9. doi: 10.1016/j.jdent.2012.10.017.

Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater. 2007 Jan;23(1):45-50. doi.org/10.1016/j.dental.2005.11.040.

Yang B, Scharnberg M, Wolfart S, Quaas AC, Ludwig K, Adelung R, Kern M. Influence of contamination on bonding to zirconia ceramic. J Biomed Mater Res B Appl Biomater. 2007 May;81(2):283-90. doi.org/10.1002/jbm.b.30664.

Dal Piva AMO, Tribst JPM, Bottino MA. Evaluation of shear bond strength and shear stress on zirconia reinforced lithium silicate and high translucency zirconia. J Oral Res 2018;7(1):30-36.doi.org/10.17126/joralres.2018.007.

Nishigawa G, Maruo Y, Irie M, Oka M, Yoshihara K, Minagi S. Ultrasonic cleaning of silica-coated zirconia influences bond strength between zirconia and resin luting material. Dent Mater J. 2008 Nov;27(6):842-8. doi: 10.4012/dmj.27.842.

Paranhos MP, Burnett LH Jr, Magne P. Effect of Nd:YAG laser and CO2 laser treatment on the resin bond strength to zirconia ceramic. Quintessence Int. 2011 Jan;42(1):79-89.

Bottino MA, Valandro LF, Scotti R, Buso L. Effect of surface treatments on the resin bond to zirconium-based ceramic. Int J Prosthodont.2005 Jan-Feb;18(1):60-5. doi.org/10.1016/j.prosdent.2005.05.011.

Shahin R, Kern M. Effect of air-abrasion on the retention of zirconia ceramic crowns luted with different cements before and after artificial aging. Dent Mater. 2010 Sep;26(9):922-8. doi: 10.1016/j.dental.2010.06.006.

Dérand P, Dérand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont. 2000 Mar-Apr;13(2):131-5.

Attia A. Influence of surface treatment and cyclic loading on the durability of repaired all-ceramic crowns. J Appl Oral Sci. 2010 Mar-Apr;18(2):194-200. doi:10.1590/s1678-77572010000200015.

Blatz MB, Sadan A, Martin J, Lang B. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling. J Prosthet Dent. 2004 Apr;91(4):356-62. doi: 10.1016/j.prosdent.2004.02.001.

Dias de Souza GM, Thompson VP, Braga RR. Effect of metal primers on microtensile bond strength between zirconia and resin cements. J Prosthet Dent. 2011 May;105(5):296-303. doi: 10.1016/S0022-3913(11)60055-3.

Manso AP, Silva NR, Bonfante EA, Pegoraro TA, Dias RA, Carvalho RM. Cements and adhesives for all-ceramic restorations. Dent Clin North Am. 2011 Apr;55(2):311-32, ix. doi: 10.1016/j.cden.2011.01.011.

Mirmohammadi H, Aboushelib MN, Salameh Z, Feilzer AJ, Kleverlaan CJ. Innovations in bonding to zirconia based ceramics: Part III. Phosphate monomer resin cements. Dent Mater. 2010 Aug;26(8):786-92. doi: 10.1016/j.dental.2010.04.003.

Yang B, Lange-Jansen HC, Scharnberg M, Wolfart S, LudwigK, Adelung R, Kern M. Influence of saliva contamination on zirconia ceramic bonding. Dent Mater. 2008 Apr;24(4):508-13. doi: 10.1016/j.dental.2007.04.013.

Angkasith P, Burgess JO, Bottino MC, Lawson NC. Cleaning methods for zirconia following salivary contamination. J Prosthodont. 2016 Jul;25(5):375-9. doi: 10.1111/jopr.12441

Feitosa SA, Patel D, Borges AL, Alshehri EZ, Bottino MA, Özcan M, et al. Effect of cleansing methods on saliva-contaminated zirconia-An evaluation of resin bond durability. Oper Dent. 2015 Mar-Apr;40(2):163-71. doi: 10.2341/13-323-L.

Yoshida K. Influence of cleaning methods on resin bonding to saliva-contaminated zirconia. J Esthet Restor Dent. 2018 May;30(3):259-264. doi: 10.1111/jerd.12369.

Zhang S, Kocjan A, Lehmann F, Kosmač T, Kern M. Influence of contamination on resin bond strength to nano-structured alumina-coated zirconia ceramic. Eur J Oral Sci. 2010 Aug;118(4):396-403. doi: 10.1111/j.1600-0722.2010.00752. x.

Tunc EP, Chebib N, Sen D, Zandparsa R. Effectiveness of different surface cleaning methods on the shear bond strength of resin cement to contaminated zirconia: an in vitro study. J Adhes Sci Technol. 2016;30:554-565. doi.org/10.1080/01694243.2015.1111833.

Quaas AC, Yang B, Kern M. Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures. Dent Mater. 2007 Apr;23(4):506-12. doi: 10.1016/j.dental.2006.03.008.

Krifka S, Preis V, Rosentritt M. Effect of decontamination and cleaning on the shear bond strength of high translucency zirconia. Dent J (Basel). 2017 Nov 14;5(4). pii: E32. doi: 10.3390/dj5040032.

Del Carpio-Perochena AE, Bramante CM, Duarte MA, Cavenago BC, Villas-Boas MH, Graeff MS, et al. Biofilm dissolution and cleaning ability of different irrigant solutions on intraorally infected dentin. J Endod. 2011 Aug;37(8):1134-8. doi: 10.1016/j.joen.2011.04.013.

Aladağ A, Elter B, Çömlekoğlu E, Kanat B, Sonugelen M, Kesercioğlu A, Özcan M. Effect of different cleaning regimens on the adhesion of resin to saliva-contaminated ceramics. J Prosthodont. 2015 Feb;24(2):136-45. doi: 10.1111/jopr.12170.

Ishii R, Tsujimoto A, Takamizawa T, Tsubota K, Suzuki T, Shimamura Y, Miyazaki M. Dent Mater J. Influence of surface treatment of contaminated zirconia on surface free energy and resin cement bonding. 2015;34(1):91-7. doi: 10.4012/dmj.2014-066.

Kim DH, Son JS, Jeong SH, Kim YK, Kim KH, Kwon TY. Efficacy of various cleaning solutions on saliva-contaminated zirconia for improved resin bonding. J Adv Prosthodont. 2015 Apr;7(2):85-92. doi: 10.4047/jap.2015.7.2.85.

Pereira Lde L, Campos F, Dal Piva AM, Gondim LD, Souza RO, Özcan M. Can application of universal primers alone be a substitute for airborne-particle abrasion to improve adhesion of resin cement to zirconia? J Adhes Dent. 2015 Apr;17(2):169-74. doi: 10.3290/j.jad.a33974.

Hussain AM, Al-Azzawi AJ. Shear bond strength between lithium disilicate ceramic and different luting cements. J Prosthet Dent 2015;3:212-217.

Gomes AL, Ramos JC, Santos-del Riego S, Montero J, Albaladejo A. Thermocycling effect on microshear bond strength to zirconia ceramic using Er: YAG and tribochemical silica coating as surface conditioning. Lasers Med Sci. 2015 Feb;30(2):787-95. doi: 10.1007/s10103-013-1433-z.

Qeblawi DM, Campillo-Funollet M, Muñoz CA. In vitro shear bond strength of two self-adhesive resin cements to zirconia. J Prosthet Dent. 2015 Feb;113(2):122-7. doi: 10.1016/j.prosdent.2014.08.006.

Ehlers V, Kampf G, Stender E, Willershausen B, Ernst CP. Effect of thermocycling with or without 1 year of water storage on retentive strengths of luting cements for zirconia crowns. J Prosthet Dent. 2015 Jun;113(6):609-15. doi: 10.1016/j.prosdent.2014.12.001.

Downloads

Published

2020-09-30

Issue

Section

Clinical or Laboratorial Research